Skip to search boxSkip to navigationSkip to main content

Compositional influence on the strength of dental porcelain

  • Philip S. Baker(corresponding author)
    ,
  • Arthur E. Clark
*Corresponding author for this work
  • University of Florida
Scholary Output:
Contribution to journal
Article
Peer-review

Abstract

This work compared the tensile strength of two glass compositions with published values of currently available dental porcelains. The influence of several variables, such as air and vacuum firing, firing temperature, surface roughness, immersion in water, and the inclusion of filter particles, on the inherent strength of the glass compositions is also discussed. The authors developed a glass frit having a tensile strength of 102.4 MPa as determined by the biaxial flexure technique. This value compares favorably with the reported strength of commercial brands of feidspathic porcelains. The strength of this glass was not significantly reduced as a result of surface abrasion or immersion in distilled water.

Publication Information

Output type

Scholary Output:
Contribution to journal
Article
Peer-review

Original language

English (US)

Pages from-to (Number of pages)

Pages 291-297 (7 pages)

Journal (Volume, Issue Number)

International Journal of Prosthodontics (Volume 6, Issue 3)

Publication milestones

  • Published - 1993

Publication status

Published - 1993

ISSN

0893-2174

Publication IDs

  • Scopus: 0027604435
  • PubMed: 8397699

Publication metrics

Metrics

Scopus
citations
Fractional count
1
Fractional count
0.50
Fractional count
1
Fractional count
0.50
Fractional count
1
Fractional count
1

PlumX

Citation count
6
Captures
9