Skip to search boxSkip to navigationSkip to main content

Effects of acid-etching on the tensile properties of demineralized dentin matrix

  • Yi Zhang
    ,
  • Kelli Agee
    ,
  • Jacques Nör
    ,
  • Ricardo Carvalho
    ,
  • Bhupinder Sachar
    ,
  • Carl Russell
*Corresponding author for this work
  • Augusta University
    ,
  • University of Michigan, Ann Arbor
    ,
  • Universidade de São Paulo
    ,
Scholary Output:
Contribution to journal
Article
Research
Peer-review

Abstract

<p>Objectives. Little research has been done to evaluate the effects of acids commonly used in adhesive dentistry, on the tensile properties of the demineralized dentin matrix. The purpose of this study was to evaluate the effects of a number of acidic conditioners on the ultimate tensile strength (UTS) and modulus of elasticity (E) of human coronal dentin matrix. Methods. Small hour-glass shaped (for UTS) or I-beam shaped (for determination of E) were prepared from mid-coronal dentin of extracted human third molars. After protecting the ends with varnish, the middle of the specimens was completely demineralized in 0.5 M EDTA (pH 7). UTS was determined by tensile stressing to failure. Modulus of elasticity was calculated from stress strain curves. The results were analyzed by ANOVA and Student-Neuman-Keuls test at the 95% confidence level. Results. Brief (ca. 1-2 min) exposure of demineralized dentin matrix to acids had no measurable effects on its tensile properties. Tenminute exposures to 2.5% and 17.5% nitric acid lowered (p < 0.05) the UTS compared to phosphate buffered saline (PBS)-exposed controls. Exposure of the decalcified dentin to 10% citric acid containing 3% ferric chloride, 10% citric acid, 37% phosphoric acid or 17.5% nitric acid containing 3% ferric chloride for 10 min had no effect on UTS. None of these acids consistently lowered stiffness. Significance. The results indicate that relatively long exposures to acids are required to alter the tensile properties of demineralized dentin. It is unlikely that the brief exposures to acids that are used in adhesive dentistry would acutely weaken the physical properties of demineralized dentin. However, long-term studies should be done to determine if such treatment increases the susceptibility of the matrix to hydrolysis.</p>

Publication Information

Output type

Scholary Output:
Contribution to journal
Article
Research
Peer-review

Original language

English (US)

Pages from-to (Number of pages)

Pages 222-228 (7 pages)

Journal (Volume, Issue Number)

Dental Materials (Volume 14, Issue 3)

Publication milestones

  • Published - 06/1998

Publication status

Published - 06/1998

ISSN

0109-5641

Publication IDs

  • Scopus: 0032082464
  • PubMed: 10196799

Publication metrics

Metrics

SciVal
FWCI
0.41
SciVal
Author count
7
SciVal
citations
13
SciVal
Paper percentile
63
Scopus
citations
Fractional count
1
Fractional count
0.14
Fractional count
6
Fractional count
0.86
Fractional count
1
Fractional count
1

PlumX, opens in new tab

Captures
47
Citation count
18

Funding Details

This work was supported, in part, by grant DE06427 from the National Institute of Dental Research, by the Medical College of Georgia Biocompatibility Group and by FAPESP grant 95/3895-9 (to RMC).
FundersFunding numbers
NIDCR
R01DE006427
FAPESP
95/3895-9