Effects of resin hydrophilicity on water sorption and changes in modulus of elasticity

  • Shuichi Ito
    ,
  • Masanori Hashimoto
    ,
  • Bakul Wadgaonkar
    ,
  • Nadia Svizero
    ,
  • Ricardo M. Carvalho
    ,
  • Cynthia Yiu
*Corresponding author for this work
  • Health Sciences University of Hokkaido
    ,
  • Hokkaido University
    ,
  • Medical College of Georgia
    ,
  • Universidade do Sagrado Coração
    ,
  • Universidade de São Paulo
    ,
  • The University of Hong Kong
Scholary Output:
Contribution to journal
Article
Research
Peer-review

Abstract

<p>As acidic monomers of self-etching adhesives are incorporated into dental adhesives at high concentrations, the adhesive becomes more hydrophilic. Water sorption by polymers causes plasticization and lowers mechanical properties. The purpose of this study was to compare the water sorption and modulus of elasticity (E) of five experimental neat resins (EX) of increasing hydrophilicity, as ranked by their Hoy's solubility parameters and five commercial resins. Methods: After measuring the initial modulus of all resin disks by biaxial flexure, half the specimens were stored in hexadecane and the rest were stored in water. Repeated measurements of stiffness were made for 3 days. Water sorption and solubility measurements were made in a parallel experiment. Results: None of the specimens stored in oil showed any significant decrease in modulus. All resins stored in water exhibited a time-dependent decrease in modulus that was proportional to their degree of water sorption. Water sorption of EX was proportional to Hoy's solubility parameter for polar forces (δp) with increasing polarity resulting in higher sorption. The least hydrophilic resin absorbed 0.55 wt% water and showed a 15% decrease in modulus after 3 days. The most hydrophilic experimental resin absorbed 12.8 wt% water and showed a 73% modulus decrease during the same period. The commercial resins absorbed between 5% and 12% water that was associated with a 19-42% reduction in modulus over 3 days.</p>

Publication Information

Output type

Scholary Output:
Contribution to journal
Article
Research
Peer-review

Original language

English (US)

Pages from-to (Number of pages)

Pages 6449-6459 (11 pages)

Journal (Volume, Issue Number)

Biomaterials (Volume 26, Issue 33)

Publication milestones

  • Published - 11/2005

Publication status

Published - 11/2005

ISSN

0142-9612

Publication IDs

  • Scopus: 22544463664
  • PubMed: 15949841
  • ORCID: /0000-0003-1947-3337/work/54796669

Publication metrics

Metrics

SciVal
citations
415
Scopus
citations
SciVal
FWCI
9.63
SciVal
Author count
13
SciVal
Paper percentile
99
SciVal
Top percentile
1
Fractional count
3
Fractional count
0.23
Fractional count
10
Fractional count
0.77
Fractional count
3
Fractional count
1

PlumX, opens in new tab

Captures
258
Citation count
545

Funding Details

The authors thank Bisco Dental Products Co. (Schammberg, IL) for the preparation of the five experimental resin blends employed in this study, and Ivoclar/Vivadent (Schaan, Liechtenstein), 3M ESPE (St. Louis, MO, USA), Tokuyama Corp. (Tokyo, Japan), Kuraray Medical Inc. (Osaka, Japan), L.D. Caulk (Milford, DE, USA) for their generous donations of their dentin bonding systems. This work was supported by Grants R01 DE04911 and R01 DE15306 from the National Institute of Dental Research (P.I. David Pashley), by Grant 10204604/07840/08004/324/01, Faculty of Dentistry, the University of Hong Kong, and by Grant 474226/03-4 from CNPq, Brazil. The authors are grateful to Michelle Barnes for secretarial support.
FundersFunding numbers
Istanbul University, Faculty of Dentistry, Department of Operative Dentistry
-
National Institute of Dental Research
-
NIDCR
R01DE015306
CNPq
-
HKU
474226/03-4