Monomer conversion, microhardness, internal marginal adaptation, and shrinkage stress of bulk-fill resin composites

  • Bruna Marin Fronza(corresponding author)
    ,
  • ,
  • Roberto Ruggiero Braga
    ,
  • Borys Mogilevych
    ,
  • Luis Eduardo Silva Soares
    ,
  • Airton Abrahão Martin
*Corresponding author for this work
  • Universidade Estadual de Campinas
    ,
  • ,
  • Universidade de São Paulo
    ,
  • Universidade do Vale do Paraíba
Scholary Output:
Contribution to journal
Article
Research
Peer-review

Abstract

<p>Objective To evaluate degree of conversion (DC), Knoop microhardness (KHN), internal marginal adaptation (IA), and polymerization shrinkage stress (PS) of one conventional and four bulk-fill composites. Methods Bulk-fill composites tested were Surefil SDR (SDR), Filtek Bulk-Fill (FBF), Tetric EvoCeram Bulk-Fill (TEC), and EverX Posterior (EXP). The conventional composite Herculite Classic (HER) was tested using both incremental and bulk-fill insertion techniques. Standardized Class I preparations (4-mm-depth) were made in extracted molars and restored with each product system (N = 5). After 1-week wet storage, restorations were cross-sectioned and DC and KHN were evaluated at four depths (1, 2, 3, and 4 mm) using confocal Raman spectroscopy and KHN techniques, respectively. Epoxy resin replicas of restorations were evaluated using scanning electron microscopy for IA. PS was determined using composite bonded to acrylic rods attached to a universal testing machine (N = 5). Results Within bulk-fill products, only SDR and FBF demonstrated similar DC at all depths, and KHN values did not statistically differ among depths, except for TEC. Neither placement method nor depth affected KHN or DC, except the DC of HER bulk-fill at 4 mm. Incrementally layered HER, and bulk-fills SDR and TEC demonstrated the lowest proportion of internal gaps. Highest and lowest PS values were measured for EXP and TEC, respectively. Significance DC with depth was not uniform among all bulk-fill materials, although no difference in KHN was found. Higher PS correlated positively with higher proportion of interfacial gaps. The incremental technique using conventional composite showed reduced gap formation.</p>

Publication Information

Output type

Scholary Output:
Contribution to journal
Article
Research
Peer-review

Original language

English (US)

Pages from-to (Number of pages)

Pages 1542-1551 (10 pages)

Journal (Volume, Issue Number)

Dental Materials (Volume 31, Issue 12)

Publication milestones

  • Accepted/In press - 02/23/2015
  • Published - 12/01/2015

Publication status

Published - 12/01/2015

ISSN

0109-5641

Publication IDs

  • Scopus: 84947578872
  • PubMed: 26608118
  • ORCID: /0000-0003-1947-3337/work/54796679

Publication metrics

Metrics

SciVal
citations
103
SciVal
FWCI
4.40
SciVal
Author count
8
SciVal
Paper percentile
98
SciVal
Top percentile
5
Fractional count
1
Fractional count
0.13
Fractional count
7
Fractional count
0.88
Fractional count
1
Fractional count
1
Scopus
citations

PlumX, opens in new tab

Captures
330
Citation count
248

Funding Details

This study was supported by The State of São Paulo Research Foundation (FAPESP) (No. 2013/05247-4 ). The authors are in debt to Dr. Francisco André Ossamu Tanaka (NAP/MEPA—ESALQ/USP) for scanning electron microscopy support, and to Mr. Marcos Blanco Cangiani for his technical assistance.
FunderFunding number
FAPESP
2013/05247-4